DescriptionWeld image of inconel superalloy after destructive tensile test.png |
English: Weld image of inconel 600 and inconel 718 superalloy after destructive tensile test. |
Date | |
Source |
"Rotary Friction Welding of Inconel 718 to Inconel 600" Department of Industrial Engineering, College of Engineering, King Saud University, Riyadh 11451, Saudi Arabia Academic Editor: Yutaka S. Sato Metals 2021, 11(2), 244 https://doi.org/10.3390/met11020244 |
Author | Ateekh Ur Rehman, Yusuf Usmani, Ali M. Al-Samhan, Saqib Anwar |
Licensing[edit]
- You are free:
- to share – to copy, distribute and transmit the work
- to remix – to adapt the work
- Under the following conditions:
- attribution – You must give appropriate credit, provide a link to the license, and indicate if changes were made. You may do so in any reasonable manner, but not in any way that suggests the licensor endorses you or your use.
- share alike – If you remix, transform, or build upon the material, you must distribute your contributions under the same or compatible license as the original.
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Thumbnail | Dimensions | User | Comment | |
---|---|---|---|---|---|
current | 20:56, 14 May 2021 | 815 × 155 (172 KB) | Xyz00030280 (talk | contribs) | Uploaded a work by Ateekh Ur Rehman, Yusuf Usmani, Ali M. Al-Samhan, Saqib Anwar from "Rotary Friction Welding of Inconel 718 to Inconel 600" Department of Industrial Engineering, College of Engineering, King Saud University, Riyadh 11451, Saudi Arabia Academic Editor: Yutaka S. Sato Metals 2021, 11(2), 244 https://doi.org/10.3390/met11020244 with UploadWizard |
You cannot overwrite this file.
File usage on Commons
There are no pages that use this file.
File usage on other wikis
The following other wikis use this file:
- Usage on en.wikipedia.org
- Usage on fa.wikipedia.org
Metadata
This file contains additional information such as Exif metadata which may have been added by the digital camera, scanner, or software program used to create or digitize it. If the file has been modified from its original state, some details such as the timestamp may not fully reflect those of the original file. The timestamp is only as accurate as the clock in the camera, and it may be completely wrong.
Horizontal resolution | 47.24 dpc |
---|---|
Vertical resolution | 47.24 dpc |